Xiamen Xiangxi New Material
Products

Book Cover Film Sheet Laminates Flat With PP Masterbatch

Author: Xiangxi Jack Lian
Book Cover Film Sheet Laminates Flat With PP Masterbatch
  • Product Details

Book cover film is a glossy BOPP sheet laminated onto printed board, so it has to stay clear, bond and unwind without blocking. A web that blocks or hazes shows as bubbles and a dull cover. Xiangxi's BOPP/CPP film masterbatch series — PP carrier grade, at 0.5–3% in the BOPP, controls COF and anti-block while keeping haze flat, so the laminate lies flat and glossy.

Why book cover film bubbles and blocks

  • Reel blocking — a tightly wound sheet blocks, so the laminator sees tension steps and the glue streaks.

  • Over-anti-block haze — too much mineral dulls the gloss cover buyers expect.

  • Nip pick — a tacky face lifts the adhesive at the nip, leaving bubbles under the print.

Lamination aids compared

AidFlatness / glossTrade-off
More mineral anti-blockDullHaze, weak bond
Surface slip coatShort-livedUneven, extra station
Line speed cutMarginalSlower, energy up
PP carrier film masterbatchFlat, glossyNo haze change

Xiangxi BOPP/CPP film masterbatch series

Product nameAppearanceCarrier resinRecommended dosage (W/W)Application scope
Xiangxi BOPP/CPP film masterbatch series — PP carrier gradeWhite pelletPP0.5–3%BOPP
Xiangxi BOPP/CPP film masterbatch series — PE carrier gradeWhite pelletPE0.5–3%CPP
Xiangxi BOPP/CPP film masterbatch series — powder gradeWhite pelletSilica0.5–3%BOPP, CPP

Which grade for book cover film sheet

  • PP carrier grade — the fit for BOPP book film; clarity and COF held for flat lamination.

  • PE carrier grade — for CPP-based laminates.

  • powder grade — for high-filler pre-mixes, not standard book film.

Processing notes

  • Add at the BOPP line throat with the resin; no pre-dry.

  • Start at 0.5% and check haze (ASTM D1003) and COF; 1–2% is usual.

  • Run a block test (ASTM D3354) on the reel before laminating.

  • Side gains: fewer bubbles, steadier nip, gloss kept.

Results to verify in your own lab

  • Haze (ASTM D1003): no rise versus the control.

  • COF (ASTM D1894): lower, steady band.

  • Blocking (ASTM D3354): clean reel release.

  • Bubbles / bond: fewer voids under the print.

Frequently asked questions

Why does my cover laminate bubble?

Surface tack lifts the adhesive at the nip; the masterbatch lowers tack and blocking, so bubbles drop.

Will it dull the gloss cover?

No — at 0.5–3% it adds no measurable haze, so the gloss stays true.

Does it affect the printed board?

It is the top film only; the board and ink are untouched.

Can I use it on a matte book film?

Yes; it disperses cleanly and does not change the matte look.

How do I balance haze and slip?

Step dosage in 0.5% increments while checking ASTM D1003 and D1894; most lines land at 1–2%.

Is it food-contact capable?

The PP carrier grade is for food-contact BOPP and ships with TDS and COA; verify your use.

Testing Xiangxi BOPP/CPP film masterbatch series — PP carrier grade on your Book Cover Film Sheet? Send us your recipe and target — we return the matched grade, TDS and a 1 kg sample within 3 working days.

Request Free Sample

Business Partner

10+Industry
200+City
500+Partners
HomeHome WhatsApp EmailE-mail
↑