Xiamen Xiangxi New Material

How do I run a film trial with the masterbatch on my line?

Published: November 18, 2026  ·  Author: Xiangxi Jack Lian
Share:

A disciplined film trial fits in one production week:

  • Day 1: pilot length at 1.5% (and optionally 2.5%) on the target layer; keep an untreated reference from the same resin lot.

  • Day 1–2: production-day tests — COF (film-to-film and film-to-steel), haze/gloss, blocking force, seal curve.

  • Day 7: repeat COF and optics after roll storage — the stability comparison is the core data.

  • Week 2: converting tests — printing, laminating or FFS pilot through your machine or a partner converter's.

Judging: pick the dosage where COF sits mid-window with stable aged readings, then lock. Send us the results — if any number is off-target, grade or dosage adjustment usually resolves it in one iteration.