Gloves come off on a climb, and the grip either holds the hand or it does not. A grip that goes shiny and slick in month two has lost the oil that made it tacky, and one that fades in the sun was never screened for UV. Xiangxi's thermoplastic silicone vulcanizate (TP-SiV) series — general moulding grade keeps a stable dry-and-wet grip feel, holds colour through outdoor exposure, and is let down to the hardness the bar diameter allows (see TDS).
Oil loss to sweat and sun — UV plus body heat drives free oil out of a cheap compound; the surface glazes and the grip that felt soft in the shop now slips.
Rotation on the bar — A grip that is not locked, or is bonded with the wrong adhesive, twists under torque and wears a polished ring on the bar.
Compression set at the palm — The palm loads one band of the grip for hours; a compound with poor recovery flattens into a flat spot the rider feels immediately.
| Route | Grip feel | Trade-off |
|---|---|---|
| Dual-density TPE with oil | Soft at first | Glazes, fades, leaves residue on gloves |
| Silicone sleeve | Excellent tack | Expensive, fragile, hard to mould graphics |
| TP-SiV general moulding grade | Stable tack wet or dry | Pattern and hardness must be tuned per bar |
| Product name | Appearance | Carrier resin | Recommended dosage (W/W) | Application scope |
|---|---|---|---|---|
| Xiangxi TP-SiV series — general moulding grade | White to off-white pellet | PP | Grade matched to hardness target — see TDS | Soft parts, trim, cushioning |
| Xiangxi TP-SiV series — soft-touch grade | White to off-white pellet | PP | Grade matched to hardness target — see TDS | Grips, skin-contact parts |
| Xiangxi TP-SiV series — sealing grade | White to off-white pellet | PP | Grade matched to compression-set target — see TDS | Gaskets, bellows, seals, pads |
| Xiangxi TP-SiV series — food-contact grade | White to off-white pellet | PP | Grade matched to hardness target — see TDS | Food and infant-contact parts |
General moulding grade at the softer end for a lock-on grip body, firmer for a thin slide-on sleeve.
For a lock-on collar, keep the collar firmer than the body so the clamp torque does not crush the grip.
For a two-shot grip with a hard core, one family for both shots removes the risk of the soft layer peeling off.
Ask for UV and colour-fastness data before choosing a bright colourway.
Mould the pattern at 0.4 mm depth minimum — shallow patterns polish smooth in a season of glove contact.
Keep the bore tolerance tight to the bar; a loose bore relies on the clamp and the grip still rocks under braking.
If bonding to an alloy bar, use an adhesive specified for low-surface-energy thermoplastics and cure it fully.
Wash-test the finished grip with sunscreen and sweat solution, not with water alone.
Wet friction: coefficient against a glove liner, dry and after sweat solution.
Colour: ΔE after 300 h xenon-arc exposure.
Set: recovery of a compressed band after 24 h at 40 °C.
Torque hold: rotation under the specified clamp torque after 100 ride cycles.
Tack comes from the compound rather than from surface oil, so it holds; confirm with a wet friction test using a sweat solution.
Yes, with pigments screened for UV; a colour that is not screened fades to a different hue than the one you approved.
No migrating oil means no transfer; that is the usual reason riders notice white marks on black gloves with cheaper grips.
A lock-on collar plus a tight bore; adhesive alone is not reliable on an anodised bar.
Yes — pattern depth and land width are the two parameters that decide whether a custom graphic still grips after a season.
Testing the Xiangxi TP-SiV series on your Bicycle Soft Handlebar Grip? Send us your recipe and target — we return the matched grade, TDS and a 1 kg sample within 3 working days.
Xiangxi New Material — A professional China manufacturer of Silicone Masterbatches and plastic additives. RoHS & REACH compliant options available.
Privacy Policy ·
AI Policy ·
Copyright ·
Sitemap
Copyright © 2016-2026 Xiangxi New Material Co., Ltd. All Rights Reserved.