Post-consumer PP and PE don't mix thermodynamically — they form separate phases with weak boundaries. Under impact, a crack travels along those boundaries with almost no resistance, so the part shatters even though both polymers are tough individually.
IBA fixes the failure mechanism:
Its compatibilizing segments locate exactly at PP/PE boundaries during melting.
The bonded interface now transfers stress, so cracks must plow through material instead of sliding along a boundary — that takes energy, and impact strength rises accordingly.
Phases disperse finer, so surfaces and mechanical consistency improve too.
Typical dosage on mixed polyolefin recyclate is 3–6%. Expect meaningful impact recovery and elongation gains; the blend won't become virgin-equivalent, but it moves from 'crisp waste' to a compound usable in crates, pallets, pipes and durable goods.
Xiangxi New Material — A professional China manufacturer of Silicone Masterbatches and plastic additives. RoHS & REACH compliant options available.
Privacy Policy ·
AI Policy ·
Copyright ·
Sitemap
Copyright © 2016-2026 Xiangxi New Material Co., Ltd. All Rights Reserved.