Xiamen Xiangxi New Material
Products

DX852A clears die drool in TPE medical tubing extrusion

Author: Xiangxi Jack Lian
DX852A clears die drool in TPE medical tubing extrusion
  • Product Details

TPE medical tubing is scrapped for black specks at the die tip and a rough inner surface long before it fails any physical test. Xiangxi's DX852A TPE-specific silicone masterbatch — PP+ carrier, dosed at 0.5–3% — clears die drool, lowers extrusion torque by 15–30% and gives the tube a clean, low-friction surface that slides in catheters and sets.

Why TPE medical tubing defects appear at the die

  • Oligomer plate-out — low-MW TPE fractions coat the die land, then drop as specks onto the tube.

  • High extrusion drag — tight tolerances need low shear; high torque fights the line speed and surface finish.

  • Surface grab — a high-COF lumen resists sliding during insertion and picks up contaminants.

Clean-surface routes for TPE tubing compared

RouteDie droolTrade-off
Slower line speedLessLower output, cost
Frequent die cleanManagedDowntime, labour
External slip sprayN/AContamination risk
DX852A masterbatchClearedNo extra line, lower torque

Which grade for this part

  • DX852A — best for PP-carrier TPE and TPV medical tubing; the PP+ carrier matches the base and keeps the lumen clean.

  • DX755A — choose it for PE-carrier TPE tube or when a silkier inner slip is wanted.

Processing notes

  • Add at the compounding stage on twin-screw; the pellet disperses without filter-screen blockage.

  • Start at 0.5% for thin-wall tube; 1–1.5% covers most medical lines.

  • Run a continuous extrusion with a specks-per-metre count, not a short shot.

  • Bonus: lower torque and steadier draw, fewer wall-thickness swings.

Results to verify in your own lab

  • Die drool (specks/m): sharply lower after a fixed run time.

  • Lumen COF: lower slip force for catheter or set insertion.

  • Extrusion torque: 15–30% lower at equal output.

  • Surface finish: smoother, fewer micro-pits under scope.

For tube extruders the real payback is run-time: fewer die cleans per shift means steadier output and lower scrap. Send 200–300 g of your TPE compound and we return the matched grade with an extrusion window and a reference run report.

Frequently asked questions

Will DX852A affect the biocompatibility of my TPE tubing?

The masterbatch is an additive; request the relevant compliance and extractables file for your device class and validate on the finished tubing with your notified body.

Does it change tube hardness or clarity?

Within 0.5–3% hardness and clarity stay within normal variation. Verify on your own tube before a regulated run.

Can I use it for catheter lumen slip?

Yes. The lower COF helps sliding during insertion; confirm lubricity and any device-specific test with your QA.

DX852A or DX755A for medical tube?

DX852A for PP-carrier TPE/TPV; DX755A for PE-carrier or when a silkier inner surface is specified.

What dosage for thin-wall TPE tube?

Start at 0.5%; most medical lines use 1–1.5%. Step up until drool clears and slip is adequate.

REACH and RoHS compliant?

Yes. Both grades are REACH and RoHS compliant, SGS tested, ISO 9001 with COA per batch.

Xiangxi TPE specific silicone masterbatch grades

Product nameAppearanceCarrier resinRecommended dosage (W/W)Application scope
DX852AWhite pelletPP+0.5–3%TPE, TPR
DX755AWhite pelletPE+0.5–3%TPE, TPR

Testing DX852A on your TPE Medical Tubing? Send us your recipe and target — we return the matched grade, TDS and a 1 kg sample within 3 working days.

Request Free Sample

Business Partner

10+Industry
200+City
500+Partners
HomeHome WhatsApp EmailE-mail
↑